Back when I restored my 69 Z, I (like most folks at the time) had them plated silver cad.

They came out very nice, and are still looking good today.

Then I read a thread on here that they SHOULD have in fact been galvanized.

Tearing down the 70 Corvette LT-1 chassis. Dust shields look about the same as the ones on my Z before plating. Dull silver color.

Question: what is the correct plating?
__________________
Don't believe everything you read on the internet ... Ben Franklin
Reply With Quote
Attachments - The Supercar Registry Used-1970-Chevrolet-Corvette-LS5-NCRS-Top-Flight-Bowtie-Award-Bloomington-Gold-Benchmark-1705499.jpg tn_IMG_0698.JPG PXL_20240113_234113654.jpg PXL_20240113_234105031.jpg
Click here to view all the pictures posted in this thread...
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT. The time now is 10:40 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.